How is differential scanning calorimetry (DSC) used in bitumen analysis?
- 该话题包含 1个回复,2 人参与,最后由 更新于 1年、 2月前 。
Answers
-
十一月 21, 2024 5:05 上午 by Yara Haddad
DSC measures the heat flow associated with thermal transitions in bitumen as it is heated or cooled. It identifies melting points, glass transition temperatures, and crystallization behaviors. DSC helps understand thermal properties, compatibility of additives, and the effects of modification on bitumen’s thermal stability and performance under temperature variations.