Interested in a colloid mill-homogenizer for polymer modification of bitumen. Want to know if the process is cold or hot.
- 该话题包含 1个回复,2 人参与,最后由 更新于 1月、 1周前 。
Answers
-
十一月 12, 2025 5:24 上午 by 山本 修平
The CLM-series mill works with hot bitumen (160-180°C). Polymers are added in molten form or pre-dissolved under controlled heating. Both SBS and crumb rubber processes are supported.