• Home
  • Products
    • TÁI SINH DẦU
      • HỆ THỐNG TÁI SINH DẦU CMM-R
      • HỆ THỐNG LỌC PHÒNG THÍ NGHIỆM СММ-0,001U
    • KHỬ KHÍ DẦU, SẤY DẦU NHIỆT CHÂN KHÔNG
      • TẢI LỌC KHỬ KHÍ DẦU CMM-0.6
      • MÁY DI DỘNG DẦU СММur-1L
      • THIẾT BỊ XỬ LÝ DẦU СММ-1Н
      • THIẾT BỊ KHỬ KHÍ CẦM TAY CMM-4/7
      • THIẾT BỊ DI ĐỘNG KHỬ KHÍ CMM-6/7
      • MÁY DẦU DI DỘNG CMM-10
    • HỆ THỐNG LỌC DẦU
      • CMM-1,0CF THIẾT BỊ KHỬ NƯỚC KHỎI DẦU
      • THIẾT BỊ LỌC DẦU CMM-4,0F
    • THIẾT BỊ SẤY DẦU ZEOLITE
      • KHAY CHỨA CHẤT HẤT THỤ ZP-260 SORBENT
    • GIA NHIỆT DẦU
      • GIA NHIỆT TRỰC TIẾP DẦU PPM VÀ GIA NHIỆT DÒNG DẦU
    • LÒ SẤY CHÂN KHÔNG
      • LÒ CHÂN KHÔNG BIẾN ÁP
    • Máy Xay Điện Từ
      • Máy Trộn AVS-100. Máy Xay Điện Từ
      • Máy Trộn Hóa Chất AVS-150
    • MÁY NHŨ TƯƠNG HÓA NHỰA BITUM
      • MÁY USB-2 NHŨ TƯƠNG HÓA BITUM NĂNG SUẤT 2 M3/GIỜ
      • MÁY USB-2 SẢN XUẤT BITUMEN NĂNG SUẤT SẢN XUẤT 8 M3/GIỜ
      • Bộ lọc bitum FB
    • MÁY BIẾN TÍNH BITUM. SẢN XUẤT BITUMEN BIẾN TÍNH
      • MÁY USB-3 HỆ THỐNG THỬ NGHIỆM BITUM BIẾN TÍNH
      • MÁY USB-3 BIẾN TÍNH BITUM CÔNG SUẤT 16 M3/GIỜ
      • USB-4 BỂ THU BITUM BIẾN TÍNH (USB-3)
    • HỆ THỐNG THỬ NGHIỆM CHẤT LIỆU NHŨ TƯƠNG BITUM
      • MÁY USB-3 HỆ THỐNG THỬ NGHIỆM BITUM BIẾN TÍNH
    • Accessories & Components
  • Globecore Tech School
    • Webinar Registration
  • Publications
  • About
  • Contacts
  • THIẾT BỊ SẤY KHÍ NÓNG: Sukhovey (MOJAVE HEAT)
  • LÒ CHÂN KHÔNG BIẾN ÁP
  • HỆ THỐNG AN TOÀN MÁY BIẾN ÁP TSS
  • HỆ THỐNG TÁI SINH DẦU CMM-R
  • KHAY CHỨA CHẤT HẤT THỤ ZP-260 SORBENT
  • TẢI LỌC KHỬ KHÍ DẦU CMM-0.6
  • TẢI LỌC KHỬ KHÍ DẦU CMM-0.6
  • Máy Xay Điện Từ

What types of contamination affect silicone oil, and how can they be prevented?

Asked: October 4, 2024 at 8:02 pm by Sonia Patel
  • This topic has 1 reply, 2 voices, and was last updated 1 year, 2 months ago by Sandra Green.

Answers

  • October 4, 2024 at 8:27 pm by Sandra Green

    Contaminations include:

    Moisture: Lowers dielectric strength and promotes degradation.
    Particulates: Metal particles, dust, and fibers can cause electrical discharges.
    Gases: Air and other gases reduce insulating properties.
    Acidic Byproducts: Resulting from oxidation, they can corrode transformer components.
    Prevention methods:

    Proper Sealing: Ensuring transformers are sealed to prevent ingress of moisture and air.
    Desiccant Breathers: Using devices that absorb moisture from the air entering the transformer.
    Clean Handling Practices: Maintaining cleanliness during oil sampling and maintenance.
    Regular Monitoring: Early detection of contamination allows for timely corrective action.

Articles by Topic

Only registered users can answer. No account? Sign up!

Ask question

GlobeCore Related Posts

plants-image

CMM-6RL Silicone Oil Regeneration Unit

plants-image

CMM-4/7 Portable Silicone Oil Degassing Unit

plants-image

Mobile Silicone Oil Processing Plant

  • Home
  • Products
  • Globecore Tech School
  • Contacts

® Copyright by - 2025 © GlobeCore

GlobeCore, Sadovskogo,14 Poltava, Ukraine, 36034

Trang web này sử dụng cookie để cải thiện trải nghiệm của bạn. Bằng cách tiếp tục duyệt, bạn đồng ý với việc chúng tôi sử dụng cookie. Đọc thêm trong Chính sách bảo mật của chúng tôi.

forum-form-logo

Sign up

forum-form-logo

Sign in

To continue log in with Google.

Google Login