Interested in a colloid mill-homogenizer for polymer modification of bitumen. Want to know if the process is cold or hot.
- This topic has 1 ข้อความตอบกลับ, 2 เสียง, and was last updated 1 month มาแล้ว by .
Answers
-
พฤศจิกายน 12, 2025 เวลา 5:24 am by 山本 修平
The CLM-series mill works with hot bitumen (160-180°C). Polymers are added in molten form or pre-dissolved under controlled heating. Both SBS and crumb rubber processes are supported.