Interested in a colloid mill-homogenizer for polymer modification of bitumen. Want to know if the process is cold or hot.
- This topic has 1 reply, 2 voices, and was last updated 3 weeks, 2 days ago by .
Answers
-
November 12, 2025 at 5:24 am by 山本 修平
The CLM-series mill works with hot bitumen (160-180°C). Polymers are added in molten form or pre-dissolved under controlled heating. Both SBS and crumb rubber processes are supported.